Inside the KU Leuven / EnergyVille test of the Denka® Platinum Plate

Instruments, method and result of the November 2022 laboratory characterisation — and what the test does and does not tell you.

Denka® TeamEnergy & power-quality engineers · Why® Group
Inside the KU Leuven / EnergyVille test of the Denka® Platinum Plate

In November 2022 the Power Electronics Group at KU Leuven / EnergyVille (Genk, Belgium) characterised the Denka® Platinum Plate. The investigators were Ir. Hassan Pervaiz, Ir. Sergio Perez and Prof. Wilmar Martinez.

Reported attenuation per plate Reported result: 13–15% (≈1.2–1.4 dB) per plate in the 25–30 MHz band. Lower bands showed smaller attenuation increasing with frequency.

Instruments

  • Agilent 4294A precision impedance analyser
  • Tektronix MDO3054 oscilloscope
  • Agilent 33500B waveform generator

Method

A stepped frequency sweep from 1 MHz to 30 MHz in 1 MHz steps on two-wire test cables, comparing HF voltage with and without plates fitted.

Result

Broadband HF voltage attenuation was confirmed across 1–30 MHz. Attenuation increased with frequency, reaching 13–15% (≈1.2–1.4 dB) per plate in the 25–30 MHz band.

What the test does — and does not — show

  • It characterises HF voltage attenuation on test cables.
  • It does not by itself measure plant-level energy savings. Those are site-specific and are established separately through IPMVP measurement and verification — see the field results.

References

  1. Laboratory evidence — Technical Portal
  2. KU Leuven ESAT / EnergyVille
  3. Field results